Stainless Steel Auger Casting for Food Machinery

Stainless Steel Auger Casting for Food Machinery

Stainless Steel Auger Casting for Food Machinery

A drawing-led stainless steel auger casting for food machinery, combining investment casting, cleanable geometry, stainless grade control, finishing and documented inspection.

  • Features
  • Capacities
  • Description
  • Factories visit
  • Benefits
  • Articles
  • Review
  • Top
Hygienic Stainless Steel Auger Casting Built to Drawing
  • Stainless Steel Auger Casting for Food Machinery
  • Stainless Steel Auger Casting for Food Machinery

A stainless steel auger moves minced food through a compact grinder, mixer or feeding system. The helical flight pushes product toward the cutter or discharge, while the hub and drive end locate the screw on the machine shaft. The part looks simple, but its cleaning route and running alignment depend on geometry that should be agreed before tooling.

Investment casting can consolidate the hub and flight into one stainless component when the helix can be released from wax tooling and the shell can support the section changes. Fabrication remains practical for very large, hollow or low-volume augers. The correct route follows the drawing, alloy, finish, inspection access and batch, not a general preference for one process.

Send a 2D drawing or sample, a 3D model if available, the stainless grade and standard, the food-contact market, the required finish, critical dimensions and inspection records. We can then review wax release, gating, machining allowance and the acceptance plan before the quotation becomes a production commitment. Contact us for details that are not shown on the drawing.

Casting Capacities and Specification Boundaries

The manufacturing route is confirmed from the auger drawing, alloy, finish and batch. Values below describe the approved project route; final dimensions and tolerances follow the drawing and governing standard.

SpecificationProject position
Manufacturing methodOEM custom manufacture to an approved drawing, model or sample
MaterialStainless steel; 304-type CF8 or 316-type CF8M families are common starting points, subject to the governing standard and application
Casting processInvestment casting for the auger geometry shown, after wax-release and shell feasibility review
Part envelopeContact us for details; no standard envelope is assumed for this part
Dimensional routeAs-cast features plus agreed machining on bore, datum faces, drive features or fit surfaces
ToleranceContact us for details; the exact casting and machining tolerances must be confirmed against the drawing and applicable standard
FinishingDeburring, cleaning, mechanical polishing and passivation as specified
InspectionChemical, dimensional, mechanical, hardness, surface and non-destructive checks selected for the project
Quality systemISO 9001 quality management; batch and inspection records per the agreed scope
Production capacityContact us for details; allocation is confirmed for the reviewed auger and order quantity

Stainless Steel Auger Casting for Hygienic Food Machinery

A stainless steel auger casting is suitable when a compact food-machinery screw can be formed as one investment-cast component and then machined, polished and verified to a drawing. The decision depends on wax release, flight geometry, hub-to-bore alignment, the exact stainless grade, cleanability and the batch volume that can support tooling. It also depends on whether the finished part can be inspected to useful acceptance criteria.

What a Stainless Steel Auger Does in Food Machinery

The auger is the rotating screw that receives product, advances it along a barrel or trough, and delivers it to the next operation. In a small meat grinder, that next operation may be the cutter and perforated plate. In a mixer or feeder, the auger may control dwell, blending or discharge rate.

What the Spiral Must Control

The buying decision covers the whole auger interface. The flight moves food, the hub transfers torque, the bore or shaft locates the screw, and the end clearances control how the assembly behaves after installation. A part can meet the drawing and still create a cleaning or alignment problem when one of those interfaces is treated as a detail.

Product movement

Flight pitch, outside diameter and surface condition influence how food moves. A rough or interrupted flight creates places where product can smear, trap or resist discharge.

Running alignment

The hub, shaft or bore, locating face and drive feature establish rotation. Runout at the flight or hub can change cutter clearance, vibration and wear even when the installed length is correct.

Cleaning access

Smooth transitions, accessible radii and stable surface finish support cleaning. A mirror finish on a geometry with sharp internal steps does not fix the cleaning problem.

For bulk food-equipment production, the buyer also needs repeatability. Two augers from the same drawing should share material condition, critical dimensions, finish route and inspection basis. That is why a useful RFQ separates cosmetic appearance from functional surfaces and identifies which readings will be recorded at first article and during production.

Why One-Piece Casting Changes the Assembly

Investment casting provides a way to create a complex stainless shape close to final form. It also brings tooling, wax handling, shell build and process-control decisions that should be reviewed before the supplier commits to a mold. If those decisions are deferred until after the order, the cheapest-looking quote may hide a geometry change, hand finishing burden or inspection gap.

Cast or Fabricate the Auger: A Route Comparison

A one-piece investment casting is strongest as a design choice when the hub, drive and helical flight can be created as a releasable pattern and the batch supports tooling. Fabrication and solid machining remain better choices when the geometry, repair strategy or lot size does not fit that model.

Do not compare the three routes by unit price alone. Tooling, machining, inspection, finishing, assembly labor and the cost of later geometry changes all belong in the same total-cost calculation. The table keeps the comparison on a common basis.

Decision Investment-cast auger Fabricated auger Solid-machined auger
GeometryGood for integral hub and complex flight when wax release is feasibleFlexible for large envelopes and separately formed flightsLimited by material removal and tool access
Joint countCan consolidate features into one partAdds assembly interfaces to control and inspectNo added joint, but requires more stock removal
ToolingWax tooling and process development requiredFixtures and forming or welding tooling may be lowerProgramming and fixturing dominate
Batch fitMore attractive when repeat volume can absorb toolingUseful for low volume or repair-oriented supplyOften suited to simple shapes or urgent low quantities
Surface routeCast surface can be machined, polished and passivatedWeld and heat-affected zones need their own finishing controlMachined finish is predictable but cost rises with removed volume
Main boundaryPattern release, shell support, distortion and section controlJoint design, distortion and inspection of every interfaceMaterial cost, tool reach and long cutting time
Choose casting when the geometry is the value.

If a one-piece stainless screw removes a difficult assembly, improves cleaning access and can still be inspected after machining, investment casting has a clear job. If the main advantage is a lower tooling bill, fabrication or machining may be the better commercial route.

A drawing review should identify the features that cannot be formed or released. A closed undercut around the flight, a deep hub cavity without access, or a section change that cannot be fed cleanly may force a design change. Those issues belong in the DFM conversation before the mold is cut, because a later correction can affect both tooling and the approved sample.

Review the Drawing Before Choosing the Route

For a small meat-grinder screw, the cast route can be evaluated around the hub, flight root, bore, drive end and end clearance. For a very large conveyor screw, a fabricated flight may keep the part practical and repairable. The product name does not decide the route; the drawing and the production plan do.

Five Drawing Features That Decide Castability

Start with a reviewable drawing

The castability review starts with the features that control pattern release, metal feeding and post-cast alignment. A statement such as “cast to drawing” is not enough when these features are open to interpretation.

Schematic of the five auger geometry review points A schematic stainless auger with numbered markers for flight envelope, flight section, hub and bore, drive feature and end clearance. Flow / product path →

Schematic for drawing review only; it is not a dimensioned drawing or a scale model of a customer part.

1. Flight envelope

Outside diameter, pitch, start count and handedness decide how the wax pattern, ceramic shell and finishing tools reach the flight.

2. Flight section and root

Edge thickness and the flight-to-hub radius control fill, cooling distortion and sharp edges that can retain product or wear quickly.

3. Hub and bore

The hub wall, bore length and datum faces determine machining access, shaft fit and the runout reference used for final inspection.

4. Drive feature

A flat, keyway, pin hole or spline must be formed or machined from a defined datum so torque transfer does not depend on a loose assembled joint.

5. End clearance

Front, rear and cutter-side clearances define the food path and rotating interfaces. They belong on the drawing before polishing or passivation is quoted.

Flight envelope. The outside diameter and pitch may look like simple dimensions, but they determine the space available for wax, shell and metal flow. A flight that is easy to machine from a solid block may still be difficult to release from tooling when the helix has a steep pitch or an undercut. The 3D model should be supplied whenever possible so the supplier can examine the actual helix rather than infer it from a few 2D views.

Flight section and root transition

A thin outer edge cools faster than the hub and can distort or become difficult to finish. A sharp root concentrates stress and can interrupt metal flow. A radius or tapered transition often helps, but its size must respect the intended screw performance, cleaning route and available space. The Casting design guide treats gradual transitions and balanced sections as basic controls because abrupt changes can create hot spots and shrinkage risk.

Hub, bore and drive end

The hub may be the heaviest section and the bore may require machining after casting. A datum plan is therefore more useful than a general note such as “bore concentric.” Identify the locating face, bore, outside diameter and drive feature that must work together. This lets the supplier plan casting orientation, machining allowance and inspection without guessing which relationship controls assembly.

Clearance and cleanability

The front edge must clear the cutter or mating part; the rear end must fit its drive and retaining arrangement. Gaps that are too small for cleaning or inspection can trap food residue, while an open transition can be easier to clean but may change product flow. Put these functional boundaries on the drawing and state whether they are as-cast or machined.

General investment-casting references place practical wall thickness at approximately 2 mm to 12 mm and wax-tooling draft at approximately 0.5 to 2 degrees. These are starting ranges, not automatic acceptance limits. A helical flight, long thin edge or heavy hub can require a different review because flow length, alloy, shell support, distortion and production equipment all affect the practical minimum.

Choosing 304-Type CF8 or 316-Type CF8M Stainless

“Stainless steel” is a family, not a complete purchase specification. For a food-machinery auger, the drawing should identify the cast grade, governing standard, heat treatment or condition, acceptable chemistry range and any required documentation.

CF8 and CF8M in Purchasing Terms

Austenitic stainless steels are common for food equipment because they combine corrosion resistance, ductility, toughness and cleanable surfaces. CF8 is broadly associated with 304-type cast stainless, while CF8M is broadly associated with 316-type cast stainless. The words “broadly associated” matter: the buyer and supplier should verify the exact grade against the applicable ASTM, EN, GB or customer standard instead of treating two commercial names as automatically equivalent.

Cast family Typical starting position What changes the decision
CF8 / 304-typeGeneral food-machinery corrosion resistance with good ductility and cleanabilityCleaning chemicals, chlorides, temperature, product chemistry, strength and applicable market standard
CF8M / 316-typeHigher resistance in many chloride-bearing or more aggressive service conditionsMolybdenum content, grade standard, heat condition, product contact and verification method
CF3 / CF3MLow-carbon alternatives where the governing specification calls for themExact chemistry, mechanical properties, weldability and project approval
Food contact is a compliance package, not an alloy sticker.

The intended food, cleaning regime, temperature, contact duration and destination market determine the evidence the buyer needs. A material certificate alone does not prove that a finished auger is approved for every food-contact use.

Name the market before naming the approval

Regulation (EC) No 1935/2004 establishes the principle that food-contact materials and articles must be sufficiently inert to prevent unsafe transfer or an unacceptable change in food composition or organoleptic properties. In the United States, the FDA regulates substances that come into contact with food under intended-use conditions and applies a reasonable-certainty-of-no-harm standard to the relevant regulatory route. The buyer should name the market and application so the correct material, extraction or migration testing and documentation can be specified.

Do not use “FDA stainless” or “food-grade stainless” as a substitute for a grade and acceptance plan. A purchaser may need the cast grade, standard, heat number, chemical composition, mechanical results, surface finish, passivation record and any application-specific conformity evidence. HULK Metal can manufacture and supply agreed records; the exact regulatory statement must match the approved project and test scope.

Keep Grade and Finish in the Same Review

For cleaning and corrosion life, grade selection also has to match the manufacturing route. A rough cast surface retains more residue and moisture than a controlled, polished surface, but polishing a marginal alloy does not turn it into a more corrosion-resistant grade. Geometry, alloy and finish should be chosen together.

From Wax Pattern to Stainless Helix

The investment-casting route turns the approved auger drawing into a wax pattern, ceramic shell and stainless casting. The sequence matters because some defects are created long before the final inspection station.

The production plan is not identical for every auger. Pattern orientation, cluster layout, gating and machining allowance are selected after the drawing and batch are reviewed. The steps below describe the typical route; each step produces information or control points that should be carried into the sample and production plan.

1

Release the drawing

Confirm the 2D/3D revision, alloy, critical features, datum scheme, machining allowance, finish and inspection requirements.

2

Build and inspect wax

Inject wax into the approved tool, cool it, remove flash and check the flight, hub, bore and drive features before assembly.

3

Assemble the cluster

Attach the wax pattern to the gating system. Small augers may be clustered; a large one may need a different layout so shell handling remains stable.

4

Build the ceramic shell

Repeated slurry and stucco layers build a shell around the pattern. Shell strength and coverage should support the flight edges and hub without trapping defects.

5

Dewax and sinter

Heat removes the wax and consolidates the ceramic shell. Shell condition is checked before pouring because a damaged mold cannot be repaired after stainless enters it.

6

Melt and pour stainless

Chemistry and pouring practice are controlled to the ordered grade. Gating and temperature are chosen to support the thin flight and the heavier hub as one casting.

7

Remove shell and gates

After cooling, the ceramic is removed and gates are cut away. Grinding and deburring prepare the auger for inspection and machining without damaging functional edges.

8
Machine, finish and verify

Bore, datum faces, drive features and critical clearances are machined as specified, then the part is cleaned, polished or passivated and checked against the inspection plan.

This sequence explains why a low price based only on cast weight can be misleading. Wax handling, shell support, gate removal, machining access and finish labor are all part of the route. The most economical design may use a slightly different radius, draft or machined feature if that change removes hand work without weakening the auger.

Cleanability: Polish, Passivate and Geometry

A cleanable auger needs all three things: a geometry that can be reached and flushed, a surface condition that does not trap residue, and a stainless surface prepared for the intended service. Polishing and passivation support the surface; they do not replace the drawing.

Set the Finish From the Food Path

The finish decision begins with the functional surface. Is the target mainly to remove burrs, improve cleaning, control food release, reduce visible scratches or create a specified Ra? These are different acceptance criteria. A decorative mirror finish on a non-critical outside surface can add cost without improving the food path, while a rough transition inside the product zone can remain a cleaning risk even when the outer surface looks bright.

As-cast + clean

Use this route when cast surface and machining condition already meet the drawing. Remove gates, grind, deburr, clean loose particles and verify the functional surfaces. State surface acceptance separately from dimensional acceptance so a cosmetic mark does not become an unreviewed reject.

Mechanical polish

Progressive abrasives reduce surface roughness and can make cleaning easier. Polishing removes material, so a tight edge or dimension may need protection. Give the required Ra, measured area and finish grade rather than only a photograph of a mirror surface.

Polish + passivation

After mechanical finishing and cleaning, passivation removes free iron and other surface contaminants and promotes the chromium-rich oxide layer. It does not fill pits, repair deep corrosion or add coating thickness. Agreement should include the cleaning sequence and inspection basis.

Mirror polishing can reach a reference Ra of 0.05-0.20 μm, but that value belongs to a controlled multi-stage polishing route with an agreed measurement method. It is not a default result for every stainless casting and should not appear as a guarantee unless the surface area, instrumentation, cutoff and sampling plan are defined.

Check the geometry before adding polish

Look for retained product at flight roots, hub steps and end clearances. If the geometry forms an inaccessible pocket, adding a bright finish may only make the pocket easier to see. A small radius change, open transition or relocated machining relief can solve the cleaning problem with less labor than extensive polishing.

The most useful drawing note separates required surfaces: product-contact flight and hub areas, sealing or locating faces, drive surfaces and cosmetic zones. Each can receive the finish and inspection level it actually needs. That prevents the supplier from applying a decorative standard everywhere and also prevents a critical food-contact surface from being treated as ordinary as-cast material.

Inspecting a Rotating Food-Contact Auger

Inspection should prove the features that make the auger work: material identity, shaft or bore fit, drive engagement, flight position, edge condition, cleanability and the specified finish. A dimensional report that omits the functional relationship between those features does not give the buyer useful evidence.

Define the Datum Before the Instrument

The drawing should define datums before the inspection method is chosen. For example, the hub face may establish axial position while the bore establishes the rotation axis. Flight outside diameter, pitch and runout can then be checked relative to that axis. Without a clear datum plan, two inspectors can produce different results from the same part.

Evidence area Typical method Buyer decision it supports
Material identityChemical composition and certificate reviewConfirms the ordered stainless family before release
Dimensional fitCalibrated gauges, CMM or drawing-specific fixturesConfirms bore, datum, drive and assembly relationships
Flight geometryOutside diameter, pitch, profile and runout checksSupports cutter clearance and stable rotation
Internal soundnessVisual plus UT, RT or another specified NDTAddresses hidden porosity or discontinuities where risk warrants
Surface and finishVisual condition, roughness and agreed passivation checkMeets cleaning and appearance requirements without substituting for geometry
Final shipmentQuantity, identification, packing and record reviewPrevents a correct sample from becoming an unverifiable batch

CMM proves a chosen set of geometry

CMM inspection is useful when many dimensions and relationships must be evaluated from one datum system. The Casting QC guide describes CMM output as measuring multiple points against a CAD model or drawing and recording measured values, nominal limits and pass/fail results. For an auger, that can include bore position, hub face location, drive feature and selected points on the flight. It does not automatically cover every food-contact surface or every internal defect.

Let the risk select the NDT method

NDT should follow risk rather than habit. Visual inspection belongs on every batch. Ultrasonic or radiographic inspection may be specified where internal shrinkage, gas porosity or inclusion risk affects the part. Liquid-penetrant inspection may help reveal surface-breaking discontinuities on suitable stainless surfaces, while magnetic-particle methods apply to ferromagnetic materials and are not an automatic fit for austenitic stainless.

Finish inspection should identify the area, the criterion and the instrument. A visual “polished” note is not the same as a measured Ra requirement. A passivation record is not the same as proof of corrosion resistance for every food chemical. Agreement should state whether the check is visual, water-break, roughness, chemical or another specified test.

Keep First Article and Production on One Record

For production, keep the first-article record as the approved baseline. During the run, check the characteristics that can drift: pattern condition, casting dimensions, bore and runout after machining, surface condition, finish condition and packing quantity. The final report should connect the delivered batch to the drawing revision and material heat.

Factory Insider: What We Review Before Quoting

In our workshop review, the most expensive surprises rarely come from the alloy itself. They come from a drawing that cannot release cleanly, a finish request that is not measurable, or a fit dimension that is discovered only after the first cast sample.

We look at the wax before the mold

A helical flight can look sound on the drawing and still tear or distort during pattern removal. We check the release direction, undercuts, sharp edges and hub depth before accepting the tooling route.

We balance the feed to the flight

The hub is a heavier section than the flight edge. We review gating and riser logic so the thin flight fills while the hub receives enough feed to reduce shrinkage risk.

We choose what will be measured

For a rotating screw, bore and datum control matter as much as the outside diameter. We settle those checks before the sample so the buyer sees the same result we do.

We also separate the finish from the geometry. If the product-contact path has a crevice or unreachable root, a bright polish will not make it hygienic by itself. We would rather adjust the radius, transition or machining relief and then apply the finish that the drawing actually requires.

This is the factory-view discipline behind the quote: find the process constraint while it is still a drawing change, define the acceptance evidence before the first sample, and keep the same datum and material record through the production batch.

RFQ Package and Common Drawing Failures

A usable auger quotation starts with a complete drawing package. At minimum, provide a 2D drawing or physical sample; add a 3D model, alloy standard, finish, inspection plan and batch whenever available.

The checklist below is a review aid, not a substitute for engineering approval. Use it to expose missing inputs before the supplier assigns tooling or estimates machining. All items remain visible without JavaScript; the script only records progress in the browser.

0 of 10 items marked for review

A common failure is a drawing that shows the outside profile but not the working relationships. Another is a finish callout with no measurement area, or a food-contact requirement with no destination market. These gaps do not disappear during production; they usually return as a sample dispute.

Can you cast an auger from a sample without a drawing?

A sample can support technical evaluation, but a dimensioned drawing is still preferred for critical fits, datums, tolerances and inspection. The sample may not preserve the material grade, heat condition or finish that the new order actually needs.

Is polishing required on every stainless food auger?

No. The need depends on cleaning access, product residue, surface roughness and buyer acceptance. Deburring and cleaning may be enough for some surfaces, while a defined polish and Ra may be necessary for others.

Can the page guarantee a food-contact approval?

No. Approval depends on the finished material, intended use, destination regulations and test scope. HULK Metal can supply agreed material and inspection records, but a blanket approval claim would be inaccurate without the completed compliance package.

Send the reviewed package with the 2D drawing, 3D model and target batch. We can then return a manufacturing route that identifies the tooling, machining, finishing, inspection and documentation assumptions behind the quote.

Quality Control: What We Test for Stainless Food-Machinery Augers

Inspection is selected from the auger drawing, material standard and food-contact risk. The production route is not considered complete until the sample and batch records show that the agreed material, geometry, surface and packaging conditions have been met.

Acceptance is a linked record

Material heat, drawing revision, critical measurements, finish condition and shipment identity should remain connected. A passing value is more useful when the buyer can tell which approved revision and batch it belongs to.

Raw Material Inspection

The ordered stainless grade and heat are checked against the material documentation. Chemical composition is verified as required before release to production. Any substitution, unclear grade or missing certificate is resolved before melting or machining begins.

Production Inspection

Pattern condition, wax assembly, shell condition, melt practice, pouring and gate removal are monitored at the points where defects can be introduced. Abnormal shell damage, filling problems or section variation is recorded and handled before the batch is accepted.

Dimension Inspection

Hub and bore relationships, datum faces, drive features, outside diameter, pitch, end clearances and runout are measured according to the approved plan. Gauge or CMM selection follows the tolerance and access. Results are recorded against the drawing revision.

Mechanical Testing

Tensile, hardness, impact or other mechanical checks are specified when the material standard or application requires them. Test frequency and specimen preparation follow the agreed standard. Results are linked to the heat or batch and are not replaced by a generic quality statement.

Surface Inspection

The product-contact flight, hub, roots and accessible transitions are checked for cracks, porosity, laps, sharp edges, embedded particles and finish defects. Surface acceptance is defined by drawing zone and function rather than by appearance alone.

Finished Product Inspection

After machining and finishing, critical dimensions, runout, surface condition and the requested finish are reviewed together. Where passivation is specified, the agreed cleanliness or water-break check and record are completed. Quantity and identification are verified.

Packaging Inspection

Packaging is checked for protection, separation, moisture control, labels, quantity and shipping marks. The packing method is matched to the auger edges and finish so transport does not create the defect that production avoided. Records close the batch before dispatch.

Ready for a manufacturability review? Send the 2D drawing, 3D model or sample, alloy standard, food-contact market, finish and inspection scope. We will return the route assumptions that need resolution before tooling.

The Foundries and Workshops Producing Your Auger

Production is coordinated through qualified casting, machining and inspection resources. Each production stage is matched to the approved drawing, stainless grade, finishing route, inspection plan and final delivery requirement for the auger project.

Why Buyers Choose HULK Metal for Food-Machinery Castings

Food-machinery buyers need a supplier who can connect drawing review, stainless material selection, casting, finishing, inspection and delivery. Our work is organized around those decisions and the records that support them.

  • Engineering Review Before Tooling

    The auger drawing is checked for wax release, flight root transitions, hub and bore access, machining allowance, gating and inspection reach before tooling starts. This review helps expose a geometry or acceptance conflict while the design can still change at low cost. Buyers receive a manufacturable route tied to the drawing, not a quotation based only on outside diameter and weight. The review also records which assumptions still need buyer approval before sample release.

  • Batch and Material Traceability

    Material certificates, chemical composition results and manufacturing records can be maintained according to the agreed project scope. Stainless grade, heat and batch identity remain connected through casting, machining, finishing and packing. That record chain supports incoming inspection, corrective action and repeat-order consistency for bulk equipment programs. It also makes a later technical question traceable to the actual delivered batch and its approved inspection file.

  • Integrated Casting and Finishing Route

    We coordinate specialized casting, machining and surface-treatment resources instead of treating each operation as an isolated purchase. Gate removal, deburring, polishing, passivation, inspection and packaging are planned in the correct order. The result is one technical route with fewer handoff gaps for the buyer to manage. The approved finish and inspection conditions travel with the part through every subcontract step.

  • Support After Delivery

    If a confirmed quality discrepancy or shortage appears, the project records are reviewed and corrective action is agreed. Options can include replacement production, replenishment, return, exchange, rework or another mutually agreed solution. Continued technical clarification and documentation support help the buyer close the issue without restarting supplier selection. The response follows the documented finding and agreed project requirements, with the next action recorded.

Further Reading on Investment Casting and Stainless Parts

These published guides help buyers compare casting routes, set tolerances, evaluate surface finish and connect machining to an investment-cast stainless part. Use them to prepare the technical questions that belong in the auger RFQ, especially when the drawing must define the working surface, datum scheme and inspection evidence before a supplier quotes tooling or approves the first sample.

Reviews on HULK Metal Casting Service
WRITE A REVIEW
leave a message
Could I Have Your Name?
How Could I Contact You More Convenient?
You can upload parameters or drawings here.
Uploading +
Could you tell me the kind of support you hope to get?